Title: | Abrasive and Fretting Wear Resistance of Refractory Cobalt Alloy Specimens Manufactured by the Method of Selective Laser Melting |
Authors: | Tarasova, T.V. Nazarov, A.P. Shalapko, Yu.I. |
Keywords: | selective laser melting;refractory cobalt alloy;abrasive wear;fretting |
Issue Date: | 2014 |
Citation: | Tarasova T. V. Abrasive and Fretting Wear Resistance of Refractory Cobalt Alloy Specimens Manufactured by the Method of Selective Laser Melting / T. V. Tarasova, A. P. Nazarov, Yu. I. Shalapko // Journal of Friction and Wear. – 2014. – Vol. 35, No. 5. – P. 365–373. |
Abstract: | This paper reports the results of comparative studies of the abrasive and fretting wear resistance of specimens manufactured by the method of selective laser melting and casting. The materials of specimens are powdered CoCrMo cobalt refractory alloy and the cast KKhS D cobalt based alloy |
URI: | http://elar.khnu.km.ua/jspui/handle/123456789/2570 |
Content type: | Стаття |
Appears in Collections: | Кафедра основ проектування |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
TRENIE I IZNOS.pdf | 2,08 MB | Adobe PDF | ![]() View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.